129
Specifications
Paper Specification
02/11/2009 TTP 7020™/TTP 7030™ Technical Manual P1003636-001
Thermal coating
Perforation
Preprinting
Thermal coating Outer side
Sensitivity Activated at approx. 68 °C saturated at approx. 75 °C.
Dynamic sensitivity 1.14 ±0.04 OD
Top coating Standard, semi or UV (if applicable)
Tear-off perforation Punching must be done from outer side (thermal coating side)
with a sharp perforation tool.
General To endure the heat developed during printing, the preprint
must meet the requirements applicable for preprinting on
paper intended for laser printing. OCR-blind ink must be used
for preprint on the inner side of the roll.
Ink used for preprinting on the thermal side must be non-
abrasive.
The ink must not smear while wound up on the supply roll or
during the printing process.
Print side One side or both sides.